I tried to print a Darth Vader pen cup using an Neofil 3D Black ABS and I obtained a strange result. It’s look like Warping but not at the buildplate interface (Buildtak at 90 °C). It seems to be a kind of Warping between every material layers…
My printer parameters was : Tnozzle = 260 °C, Tplate = 90 °C, Fan = 50 %, Flow = 107 %, Retraction = 4.50 mm
It looks like delamination are you using a enclosed printer? Changes in temperature / draughts can cause layers to split. You might also want to try lowering your temperature of the abs.I print abs at about 220-235 but that’s dependent on print speed and filament.
The part is suffering from delamination, which means the temperature might be fine, but the speed too high to allow the layers to stick together properly.
I have printed much bigger parts without an enclosure, and not suffered any noticeable warping, so my conclusion is that the high bed temp (I print at 110C) is needed to keep the part sticking to the bed (I use ABS juice on regular float glass).
So, try printing a lot slower. It will allow the top of the previous layer to melt slightly into the bottom of the fresh layer. Also, 0.2mm layer heights or smaller will help, since the previous layer will be heated up more.
I am using a standard Ultimaker 2+ so my printing area is not enclossed.
For the other missing parameters, I print at 30 mm/s (so I think it’s not too high) and 0.2 mm layers height.
I will try too print it again without cooling and maybe by decreasing nozzle temperature. Not shure a lower temperature will give a better result because I think that temperature helps layers to stick together… Why do you think about that ?
Moreover the file seems good, I already print this pen cup with really good results using PLA, Nylon and also other ABS…
Thank’s for your help, I will send you the result of the second try
Fantastic advice so far. Just to clarify though - the problem is that your layers aren’t sticking together well enough meaning the printed layer isn’t melting the layer below. The simplest fix is to turn off the fan but then you don’t get good overhangs. To get good overhangs you need either some fan (but enclose the printer) or you need to lower the temp - that’s why people say to lower the temp - lowering the temp won’t help layer adhesion but it will help your overhangs without needing to use so much fan. It takes about 100 prints to get really good at printing PLA consistently. It takes another 100 prints to then get really good at printing ABS. Enclosing the printer is really very easy with the UM2. Put some saran wrap on the front. Put a box on the top - the type of box that holds printer paper is the perfect size - it has extra space in the back for the bowden already. With that much sealing you should get air up to about 40C. Don’t go much hotter than that without moving the steppers outside the printer.