  • There’s a couple of things I can see as potentially being the problem here. 1. Partial block of the barrel and nozzle. One of the simplest ways to clean this out is heating it up and using a toothpick, dunking it in and pulling it out until it comes out clean. May need multiple toothpicks, be caref…

  • Going from memory as it was almost over a year ago since I put MadeSolid PET+ through my Rep2 (4th Gen). I was using their black PET+, temp was at or around 230C-235C on a glass plate with a thin spread of UHU glue for adhesion. I don’t think I slowed the print speed down, though it could help. I al…