should not, some % alcohol (ethanol) did it once faster here, but tap water is enough
-
Hello Obelix, the layfomm 40 is the softest version (you wrote falling apart) , layfomm60 is more stiff, both need some periods of fresh water for best rinsing results, yes PVA sticks, it´s also used as glue, best Kai
-
- Formfutura / NL - www.imprimante3DFrance.com - Matterhackers / USA - Orbi-Tech / Germany - see my own offers at ebay
-
what the price and what dealer sells it? Kai
-
Hi Community, @Brian asked me to tell something about the #POROLAY series. POROLAY is totally different to homogene (100%) materials as flex PLA or other flexibles. After printing your object in the same way you do it with other stiff filaments you rinse your object for 1-3 days in water. But pl…
-
Hi Brian, the POROLAY series ist totally different to homogene (100%) materials as flex PLA or other flexibles. After printing your object in the same way you do it with other stiff filaments you rinse your object for 1-3 days in water. But please read here some extracts, and open later the attac…