Go to homepage
21 / 23
Sep 2015

Looks like holtane posted the same idea about the humidity as I was typing my reply. Now that I think about it more, I was focused on the two weeks away. Depending on how/where you store your filament, it could have slowly been absorbing moisture prior to the vacation as well. Filament storage is something easy to get sloppy about since it doesn’t usually matter much if you’re in a climate controlled environment and actively using the printer. I have some stored in a plastic tub with desiccant but a few just out on the table next to the printer. Now that I’ve said all that, I’ve never actually had issues with humidity myself yet but have noticed that some brands seem to produce more consistent prints than others. You didn’t mention the type of material and whether or not the white and orange were the same brand. That could be a factor.

I actually had a different filament out at the time (forgot about it) and the white was in a closed cardboard box. I’m testing a different filament now to see if there is any difference.

I suspect moisture in the filament the only downside to abs is its hydroscopic quality. I’m still using stock software in my 1.0 and I had a similar issue I checked everything ended up tearing the whole machine apart screw by screw and came across cracks in the factory bearing supports when the machine reached temp the cracks would open and cause poor quality prints. I printed a couple bearing holders from the davinci section on thingiverse. I’ve been thinking of loading repetier but I’m still a little timid on the software side of things.

It looks like a filament issue, if it has been left idle for 2 weeks and has possibly absorbed moisture then the filament wont bond properly, which is what is looks like here. You can bake the filament in the oven to dry it out at a low temperature or use a low setting hairdryer. It can happen quite easily but isnt a well known problem. Thats assuming like you said you levelled the bed etc

Have you just started using the white filament ?

  • have you measured and checked the diameter of the filament
  • updated the filament diameter in the settings
  • tried increasing/decreasing the extruder temperature to get better flow

that’s all i can think of off the top of my head at the moment

Try another filament spool - the voids are symptomatic of filament that has absorbed moisture from the air. You extruder drive gear could also be a problem here - it may have bits of plastic embedded in the teeth which causes the filament to flow inconsistently. Check and clean with the small wire brush. The drive gear idler is also a problem spot. It wears and gets sloppy on the shaft. I actually installed ball bearings into mine.

I live in Louisiana. The biggest problem I run into is humidity. I place my spools in a ziplock bag with a little bit a desiccants that I bought from Lowes. This is what I suggest to do.

I have a big problem with nylon. I put it in a bag for 24 hours and the next day it is printing like a champ. After a week or so in the bag you will see a pool of water that it is collecting. Tons of water is stored in the plastic.

Try this out and let me know if it works for you.

what size ball bearings did you use in the idler? I have been packing mine full of grease lately which seems to help, but switching to a bearing would be the best thing to do.

I had same problem. this is what I did to fix it.

1. Clean nozzle with provided wire.

2. load filament, let some plastic extrude.

I did 3 times to make sure is total clean.

I’ve put my filament in the oven for about 2 hours to dry it out. That had no effect on the print quality. Did the same (a bit longer) for another spool, also without any effect. Although I have to agree with all advice here that the filament really isn’t sticking properly.

Maybe the temperature of the nozzle isn’t correct?

There was one setting that had a big effect on the print quality. Turning infill before perimeters off. To my surprise though because before turning this setting on actually improved all my prints dramatically.

I added a pic of the results so far (also showing a whole new problem), sorry for the poor quality (new phone broke).

Left is what it printed like up to 3 weeks ago.

The middle one 3 weeks later without making any changes (besides cleaning the print nozzle and leveling the bed).

On the right is the current result.

Besides the top part getting messed up (does that every time, but only with this model, no clue yet what causes it) it looks pretty similar to the original old print. The print is still a little bit zigzagging in the Z axis, but definitely acceptable. The problem I have is the seems, they are pretty wide and go inwards while the original goes out. With this white filament the shading makes them very visible.

Is there any way to tweak this and get them seems tighter and maybe oozing(?) out a little bit.

Thanks for all the advice so far, I still have to look into some of the more hardware related solutions, because I have no idea where I can even find most of the parts that are mentioned :stuck_out_tongue:

It looks like your z layers aren’t the right height, try flashing the firmware or printing something with a defined height and measure it…

Try drying your material in an oven overnight at 60 C. I think this is a moisture issue.

Very unusual problem! Have you inspected your extruder gear? Perhaps there is an obstruction or noticeable wear. Also I have found when changing filament that I’ve had to increase or decrease the temperature as not all filaments are the same quality.

Apart from that I would suggest reducing the distance between your extruder nozzle and heated bed just a tiny bit. Good luck!

2 months later