Printing my die, I changed the first layer to 90% and it is working great I really think that was my problem, I think :slight_smile:

In my opinion, I think you should go with .3 for your initial layer thickness. It for some reason is what Wanhao profiles are showing. It is what I use for PLA, HIPS, and ABS, and I usually get good results. I know that the 3dprinterwiki.info web site says otherwise, but try both and see which one fixes your air bubbles.

I have found if I Set extruder to 205c and the printbed to 70c it seems to lay down filament fine but the edges of the raft curl up not all of them but like one or 2. Then I was printing a Microsoft Band (stand) it printed fine (except for the raft lifting in the corners) then about 3/4 the way up the neck the neck was all messed up like it had been chewed on, I tried this twice with different results but both times the neck was messed up to a degree, Im also finding that When the filament covers over the filler (triangles) it doesnt cover smoothly or properly, what would cause this?

sembra che il piano non sia livellato bene, dove fa le bolle sei più distante dal piano e quindi il materiale non è spalmato bene e lo strato risulta più grosso e non ancorato al letto caldo.

Prova a fare il primo layer più basso con il piano livellato meglio. Porta in temperatura il piatto caldo prima di fare il livellamento anche il vetro si deforma con il calore e si deve assestare.