I have tried everything i can think of but i am still getting ooze to the point that most of my travel lines end up being single thickness walls. I am printing in PLA with a prusa i3. Temps i have tried are anywhere between 195-200, and retraction up to 5mm, and still getting the ooze. Any suggestions?
What brand of filament? What are your retraction settings for vertical lift and speed, what is your travel speed set to? Also check here: Print Quality Guide | Simplify3D Software 4
Sorry it took so long to get back, been busy. The brand filament is “inland” yes it is cheap stuff, but i have been printing with this brand for over a year and have never had this issue. My settings are:
Retraction = 3 - 10mm
Retraction Speed = 20 - 50
Z Lift = 2mm
Nothing has changed, i never used to have any of these settings and my parts came out perfect, now my parts require so much “cleaning up” i am tempted to just throw them in the recycle pile.