This was a calibration print. I set a print speed of 40 mm/s but it slows down to about 10 mm/s if the layer print time is below 30 sec. Also I can adjust the extrusion percentage lower but the i have a problem where the walls would be to thin and not printed at the desired thickness. I will keep trying
it is a smooth rotation then its stops for a fraction of a sec. I don’t think i have noticed it jump.
Layer height is .25, .4 nozzle, 1.75mm filament, at 40 mm/s print speed(Slowed down to 10 mm/s if layer print time is under 60 sec), heatbed at 60 c, and hotend at 220 c (I use a B3 Pico and due to the design it has to run a bit hotter or else it jets jammed)
This object was PLA but also happens with ABS. Also i have used ninjaFlex and it prints out perfectly. I believe it does so becuse of the unique way ninjaFlex prints out and creates a small pressure in the melting chamber so it doen’t matter if the motor start and stops, as long as the delay is not to long.
Honestly I believe it might be a micro stepping issue in the Marlin Firmware but I have had a difficult time finding and info doing google searches.