I bought a CR-10 a while back and since having it I have only ever managed 2 successful prints (which are really nice). I know I’m messing something up here. I’m printing at 200 degrees, with a 60 degree bed and PLA. My prints seem to either be running themselves over and tearing off in the first layer, or, coming off the print bed about half way through. I have been trying to print with a brim, but, it tends to tear the first layer off. Any suggestions?
Spizmar
2
I just got a new cr-10
The only way move works is if I use a raft, so you could try that.