Getting ready to try some nylon. Looking for any advice including brand and where you got it. I am in the US so that will factor in on a vendor I guess.
Printer will be a Flashforge Creator Pro with Micro-Swiss all metal hot ends.
Taulman 680 is my favorite. If you get good layer adhesion, it is indestructable.
Also, since you have microswiss, immediately get some PETG!!!
I have some frosted red that is KILLER!
Also on the micro swiss. PTFE acts as an insulator, so what you are used to printing temperature wise may change a little.
ABS seems to flow ok, but I had to lower my temps on PLA because I would get heat creep up the nozzle and it would get soft at the top, preventing a good push, and thus “clogging”…
With ABS, btw, you can crank up your speeds!
Have fun. Also, follow the direction for the upgrade exactly. Dont overtighten. Use the thermal material!
I run microswiss in one extruder on each of my dual extruder printers, since I am very happy with the stock extruder, except for the fact it cannot go above 230o.
Perry, I do have a new issue since installing the MS hot ends. When doing a calibration cube (PLA) and setting the start point to specified I get what looks like under extrusion right exactly on the corner edge. It isn’t like the usual where it drags part way across the first side but it more looks like the corner was cut off just slightly or the corner looks “pitted”.
I’ll post a picture later when I can.
Thought I would mention it since you use the MS ends!!
Yeah, it popped and sizzled right out of the bag. I read reviews on Amazon with the same issue, but decided to take a chance. My buddy ordered a roll a few weeks later with the same issue. And yup its taulman. The original clear color faded to yellow.