Jun 2017

Here is my print. The side with the fins feels really smooth. Every surface feels spot on, vertical walls and the horizontal floor.

The other side, where the support was, as I’ve said feels a bit coarse, you can feel the gaps between the lines, especially with your fingernails.

And the really rough edge on top of that side is the result of supports being too close and me not having proper tools. I don’t know why, but even though I’ve used X/Y distance and minimal distance to be 0,5 mm, it got really close to the print here. But there is also an option that was selected “Z overrides X/Y” or something like that, so maybe that got to do something with it.

Oh, and this was printed with 0,15 layers - 0,2 mm first layer. First layer temp. 215 °C, other layers 205 °C, bed temp. 60 °C