RogerDS
1
My brother just checked an earlier 3D print from a Flash Forge Pro: it was the knot, and it just started falling apart.
Should I set the extruder temperature hotter? That seems the logical thing to do which, would,maybe make it stick together better.
1 Like
What material, what extruder temp, what bed temp, print speed and slicer?
1 Like
Perry_1
3
as @wirlybird said, more information would be helpful.
Post a picture, which would help us alot in analyzing.
I would lean towards underextrusion, not temperature.
Pla? Abs? Temp? Resolution? Print speed?
RogerDS
5
The filament type is PLA. The extruder temperature was 120. The bed temp was 110. And the print speed was 90.
Basically; all the default settings. We do not change the setting much because of not knowing exactly how that would effect the print-out.
Roger at RDS2@Q
Perry_1
6
PLA recommendation:
Extruder temp between 190-230.
Print speed 30-60mm/s standard until you get it dialed in.
Heated bed temp 55-60.
RogerDS
7
Wow, thanks.
I hope this solves all the problems.
Blessings to you
Roger