Go to homepage
1 / 12
Mar 2016

That’s good to know thanks ! Oddly, this information cannot be clearly found on their website.

To clean it they recommend a window cleaner like Windex, or acetone.

Did you managed to print on “cold” bed ?

Printbite should have made this more clear that a heated bed is require.

4 months later

Hi

Sorry for the long delay in updating this thread.

For me the PrintBite worked on the Printrbot simple metal without a heated bed.

I had to increase the temperature of the PLA to 210 degree. In some cases when printing at 0.1 mm I use a thin layer of

pritt stick glue, which help with adhesive.

I’ll keep experimenting with different PLA & lower adhesive.