Hi Filemon,

I hope all is good!

Maybe you can send me an email…

Cheers,

Peter

C

Some of our customers have had good results with the MadeSolid FireCast resin with the Form1 for casting.

Yes. Form 1+ with the castible resin is very good. I run about 12 rings a week for casting, and the results are excellent. The detail is good down to .3mm and the burnout is good.

4 years later

very nice casting.
i did some 18kt gold samples casting with de purple wax and form 2, the results : 70% o.k.
i would like to reach 90% satisfaction

Can you tel me witch kiln you use?
Some guys say you need to have airflow so the gases can escape better…
I use a old kiln…