4 / 19
Nov 2015

Here is a picture of the downside of a cap, on the right are the supports. As you can see, they came out in one block and the flat surface is pretty clean. Unless it’s a really intricate shape, I don’t see the need for washable supports. Unfortunately, we can’t use simplify3d or any gcode generator on cubes. The printer, the chips, software… everything is meant to waste their overpriced filament and justify their expensive ultrasonic tank. The most I have been able to do is lower down PLA temperature (set by default at 210C which I find very high for small or detailed elements particularly on a enclosed chamber) and that helps a bit to improve the print quality. I’d print all the elements in your models separately so they all come out nice and clean. Printing it in straight position requires a lot supports for those flat overhangs and in the picture looks like there is very little space to reach out to them. Maybe you could try to rotate it to the side, like in your etd197 pic, so all those flat floors won’t require supports and only the pillars and small elements will be overhangs.

Most excellent print work. It may be I could utilize your machines. I will submit a file for estimate.

3 months later

This is great.

I have a cube trio. Using Nylon and INF with the normal settings.

I havent been able to print anything with INF. My extruder keeps klogin and the one with nylon the material comes like with bubbles. Can you plesase help me.

Thank you

AD

One of the first INF cartridges I used, failed. It was determined that the INF was defective. Also, unrelated to the defective cartridge, if your extruder comes back with a filament error, it is possible the remaining previous material has jammed the extruder. I have not tried nylon yet. Have you used Simplify 3d with your machine yet? Have you ever removed an extruder and cleared a jam?

5 months later

INF material are very sensitive to moisture , I tried to remove it using an oven but its impossible. I recommend to deinstall de cartridge from printer if it don’t will be used for several days and store in a closed bag with silica. I live in buenos aires mean 70 % of humidity… Nylon are also vey hygroscopic but in this case there are solution, you need to remove the moisture in a 50…60 C oven for at least 6 hours.

Regards, Patricio