I did not get the problem… but I have good results with a Replicator 2 and those parameters (perhaps could help):

  • Material: PLA
  • Raft
  • No Support
  • Profile: Standard
  • Infill: 20%
  • Number of shells: 3
  • Layer height: 0.15mm
  • Temperature: 220°C (really depends of your filament)
  • Speed while extruding: 30mm/s
  • Speed while traveling: 90mm/s

The process is quite slow (about 5 hours for a case) but the result is really great.

Good Tip is print slower at this section. 20mm/s I use and temperature as low as possible. I use 200 degrees.

And use good filament, I’ve a china no name filament and thats a mess. Printing with 205 degress causes filament blocking cause it doesn’t melt correct and with 208 degrees it flows away.

I current use for these cases colorfabb.

Good Tip is print slower at this section. 20mm/s I use and temperature as low as possible. I use 200 degrees.

And use good filament, I’ve a china no name filament and thats a mess. Printing with 205 degress causes filament blocking cause it doesn’t melt correct and with 208 degrees it flows away.